Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 152 °C | 306 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Crystallization Temperature | 152 °C | 306 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Crystallization Temperature | 152 °C | 306 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |