| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 67.0 - 132 °C | 153 - 270 °F | Average value: 120 °C Grade Count:54 |
|
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
|
|||