Polymer Property : Vicat Softening Point = 482 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 195 - 250 °C
383 - 482 °F
Average value: 208 °C Grade Count:57
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Vicat Softening Point 228 - 250 °C
442 - 482 °F
Average value: 237 °C Grade Count:12
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Vicat Softening Point 200 - 250 °C
392 - 482 °F
Average value: 245 °C Grade Count:24
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Vicat Softening Point 200 - 250 °C
392 - 482 °F
Average value: 234 °C Grade Count:15
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..