Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 94.0 - 245 °C | 201 - 473 °F | Average value: 163 °C Grade Count:4 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Vicat Softening Point | 91.0 - 245 °C | 196 - 473 °F | Average value: 130 °C Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Vicat Softening Point | 230 - 245 °C | 446 - 473 °F | Average value: 241 °C Grade Count:4 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Vicat Softening Point | 180 - 245 °C | 356 - 473 °F | Average value: 202 °C Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |