Thermal Properties Metric English Comments
Vicat Softening Point 165 - 220 °C
329 - 428 °F
Average value: 206 °C Grade Count:23
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Vicat Softening Point 165 - 220 °C
329 - 428 °F
Average value: 208 °C Grade Count:18
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Vicat Softening Point 217 - 220 °C
423 - 428 °F
Average value: 219 °C Grade Count:3
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Vicat Softening Point 215 - 220 °C
419 - 428 °F
Average value: 219 °C Grade Count:8
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Vicat Softening Point 150 - 220 °C
302 - 428 °F
Average value: 194 °C Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Vicat Softening Point 210 - 220 °C
410 - 428 °F
Average value: 217 °C Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Vicat Softening Point 128 - 220 °C
262 - 428 °F
Average value: 183 °C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..