Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 75.0 - 108 °C | 167 - 226 °F | Average value: 95.5 °C Grade Count:98 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Vicat Softening Point | 82.8 - 108 °C | 181 - 226 °F | Average value: 97.7 °C Grade Count:72 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |