Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8278/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Vicat Softening Point | >= 320 °C | >= 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/GF/14 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/BK PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7373 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Chemical and hydrolysis resistan.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Vicat Softening Point | 320 °C | 608 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |