Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 305 °C | 581 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Vicat Softening Point | 305 °C | 581 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Vicat Softening Point | 305 °C | 581 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Vicat Softening Point | 305 °C | 581 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Vicat Softening Point | 305 °C | 581 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7107 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |