Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | >= 230 °C @Load 5.001 kg |
>= 446 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ F35 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | >= 230 °C @Load 5.001 kg |
>= 446 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ QF2515 Nylon 66,Mineral and Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | >= 230 °C @Load 5.001 kg |
>= 446 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66.6 C12^F30 Nylon 66/6, Glass Fiber, Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 230 - 252 °C | 446 - 486 °F | Average value: 244 °C Grade Count:3 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Vicat Softening Point | 230 - 255 °C | 446 - 491 °F | Average value: 248 °C Grade Count:5 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Vicat Softening Point | 230 °C | 446 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | >= 230 °C @Load 5.10 kg |
>= 446 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Vicat Softening Point | 230 °C | 446 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 230 °C @Load 5.10 kg |
446 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Vicat Softening Point | >= 230 °C @Load 5.10 kg |
>= 446 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Vicat Softening Point | 230 °C @Load 5.00 kg |
446 °F @Load 11.0 lb |
|
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GS 30 HWCP 30% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | B/120; ISO 306 |
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 230 °C @Load 5.10 kg |
446 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9230CS PET (Europe-Africa-Middle East) 15% GF PET Injection Moulding grade, Heat and Color Stabilised, for light colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 230 °C @Load 5.00 kg |
446 °F @Load 11.0 lb |
|
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |