Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 227 °C | 440 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |