Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 220 °C | 428 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Vicat Softening Point | >= 220 °C @Load 5.001 kg |
>= 428 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ F15 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 220 °C | 428 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |