Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 218 °C | 425 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Vicat Softening Point | 218 °C | 425 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |