Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 214 °C | 418 °F | ISO 306/B50 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |