Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 210 °C | 410 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 6 GF 25 Polyamide 6, 25% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 25% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Vicat Softening Point | 210 °C @Load 5.001 kg |
410 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYshine PBT D223 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | >= 210 °C @Load 5.001 kg |
>= 410 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ Nylon 66 Information provided by Polykemi AB |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Vicat Softening Point | 210 - 225 °C | 410 - 437 °F | Average value: 216 °C Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B |
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B |
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Vicat Softening Point | 210 °C | 410 °F | B |
Plastcom SLOVASTER® B1 GF 20 000/1 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticit.. |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Vicat Softening Point | 210 °C | 410 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
Vicat Softening Point | 210 °C @Load 5.00 kg |
410 °F @Load 11.0 lb |
|
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe.. |
|||
Vicat Softening Point | 210 °C @Load 5.00 kg |
410 °F @Load 11.0 lb |
|
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Vicat Softening Point | 210 °C @Load 5.00 kg |
410 °F @Load 11.0 lb |
|
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Vicat Softening Point | 210 °C | 410 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 210 °C | 410 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 210 °C | 410 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East) Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used .. |
|||
Vicat Softening Point | 210 °C | 410 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Vicat Softening Point | 210 °C | 410 °F | 50°C/h 10N; ISO 306 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NB40 GR20 NL XA70 PA6, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced 15% Glass fiber reinforced and 25% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the followi.. |
|||
Vicat Softening Point | 210 °C | 410 °F | ASTM D1525 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF10 GB20 Polyamide 6 - Glass Beads Reinforced 10% Glass fiber and 20% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Vicat Softening Point | 210 °C @Load 5.00 kg |
410 °F @Load 11.0 lb |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Vicat Softening Point | 210 - 220 °C | 410 - 428 °F | Average value: 217 °C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |