Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 196 °C | 385 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Vicat Softening Point | 196 °C | 385 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Vicat Softening Point | 196 °C | 385 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Vicat Softening Point | 196 °C | 385 °F | B 120; ISO 306 |
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6 Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr.. |
|||
Vicat Softening Point | 196 °C | 385 °F | B/50; ISO 306 |
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In.. |
|||
Vicat Softening Point | 196 - 215 °C | 385 - 419 °F | Average value: 203 °C Grade Count:5 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |