Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 194 °C | 381 °F | ASTM D1525 |
Network Polymers NPP 50-0863 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Vicat Softening Point | 194 °C | 381 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 194 °C | 381 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 194 °C | 381 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |