Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 178 °C | 352 °F | B |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Vicat Softening Point | 178 °C @Load 5.001 kg |
352 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYshine PBT D201 PBT Information provided by Polykemi AB |
|||
Vicat Softening Point | 178 °C @Load 5.001 kg |
352 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYshine PBT D401 R PBT, Medium Viscosity Information provided by Polykemi AB |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 178 °C | 352 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 178 °C | 352 °F | B50 (50°C/h 50N); ISO 306 |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Vicat Softening Point | 178 °C | 352 °F | |
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |