Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 171 °C | 340 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Vicat Softening Point | 171 °C | 340 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Vicat Softening Point | 171 °C @Load 1.00 kg, Thickness 4.00 mm |
340 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Vicat Softening Point | 171 °C @Load 1.00 kg, Thickness 4.00 mm |
340 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Vicat Softening Point | 171 °C | 340 °F | ASTM D1525 |
PlastxWorld Veroplas PA2002 Nylon 6 general purpose, unfilled, impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Vicat Softening Point | 171 °C | 340 °F | ASTM D1525 |
PlastxWorld Veroplas PA2002HI Nylon 6 general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Vicat Softening Point | 171 °C | 340 °F | ASTM D1525 |
PlastxWorld Veroplas PA2002MI Nylon 6 general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Vicat Softening Point | 171 °C | 340 °F | ASTM D1525 |
PlastxWorld Veroplas PA2009L Nylon 6 general purpose, super lubricated injection molding gradeInformation provided by PlastxWorld Inc. |