Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Multibase Nylex™ 2185 FR V0 Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Vicat Softening Point | 166 °C @Load 1.00 kg |
331 °F @Load 2.21 lb |
|
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 166 °C | 331 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1010G30 HB Polycarbonate, 30% Fiberglass Reinforced Information provided by Ravago. |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Vicat Softening Point | 166 °C @Load 1.00 kg |
331 °F @Load 2.21 lb |
|
Polykemi AB POLYfill PPH GF5040 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced Information provided by Ravago. |
|||
Vicat Softening Point | 166 °C | 331 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |