Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525B |
SABIC PP 518P Polypropylene Homopolymer for Fiber Applications Product Description: PP 518P is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518P has the following features:Consistent processabilityGoo.. |
|||
Vicat Softening Point | 152 °C @Load 5.001 kg |
306 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYform POM C M270 Polyoxymethylene Information provided by Polykemi AB |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
PolyMirae Moplen EP540S Injection Molding Grade Polypropylene Moplen EP540S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540S is a block copolymer particularly suitable for injection.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
PolyMirae Moplen HP420J BDDP Film Grade Polypropylene Moplen HP420J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP420J is a homopolymer particularly suitable for BOPP (Tender) fi.. |
|||
Vicat Softening Point | 152 °C | 306 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC H7630 Polypropylene, Homopolymer Features: Seetec H7630 is designed for the extrusion of continuous filament (CF) & bulk continuous filament (BCF) fibers and staple fibers. This grade is characterized by medium MWD, with anti-gas f.. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 1710 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 152 °C | 306 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP STAT-LOY ZF3021 PPE+PS (Europe-Africa-Middle East) LNP* STAT-LOY* ZF3021 is a compound based on PPE + PS Blend resin containing Glass Fiber. Added features include Antistatic, Flame Retardant. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ASTM D1525 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Vicat Softening Point | 152 °C @Load 5.10 kg |
306 °F @Load 11.2 lb |
A50; ISO 306 |
Borealis HD204CF Polypropylene HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru.. |
|||
Vicat Softening Point | 152 °C @Load 1.02 kg |
306 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis HD234CF Polypropylene HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 10N-50°C per hour; ISO 306 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 10N-50°C per hour; ISO 306 |
Total PPH 7062 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7062 is an antistatic homopolymer.ApplicationATOFINA Polypropylene PPH 7062 is intended for injection molding applications of boxes, closures and household articles. Inform.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
120°C/hr; ASTM D1525 |
Diamond Polymers NPP25-0120B GF15 Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 TF4 POM Tribological modified grade with addition of 20% PTFE, with very low coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 520 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 152 °C | 306 °F | 10 N; ASTM D1525 |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |
|||
Vicat Softening Point | 152 °C | 306 °F | -1kg; ASTM D1525 |
Braskem CP 405 XP Injection Molding Polypropylene Applications: Caps for soft drinks. Information provided by Braskem |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 220 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 430 N30 Polypropylene Copolymer Good surface appearanceInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C @Load 1.02 kg |
306 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem H 203 HOMO Polypropylene Homopolymer H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low .. |