Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 129 °C | 264 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS PC+ ABS General Purpose Non-FR |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Vicat Softening Point | 129 °C | 264 °F | ISO 306/A50 |
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D 1525 |
NOVA Chemicals Sclair® 2906 HDPE Injection Molding Resin NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Excellent toughness and impact resistance, High stiffness, Excellent processing stability, High GlossAdditives: .. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ISO 306/B50 |
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi.. |
|||
Vicat Softening Point | 129 °C | 264 °F | |
Covestro Bayblend® T 85 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Vicat Softening Point | 129 °C | 264 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA TW-18B2 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Vicat Softening Point | 129 °C @Load 1.02 kg |
264 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem Prisma 3410 RACO Random Polypropylene Copolymer Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent pro.. |
|||
Vicat Softening Point | 129 °C | 264 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Vicat Softening Point | 129 °C @Load 1.02 kg |
264 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem IE59U3 HDPE Injection Molding Polyethylene Homopolymer IE59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength, good pro.. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 129 °C | 264 °F | ASTM D1525 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |
|||
Vicat Softening Point | 129 °C | 264 °F | 10 N; ASTM D1525 |
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con.. |