Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 115 °C | 239 °F | STN EN ISO 306 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Vicat Softening Point | 115 °C @Load 5.001 kg |
239 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 115 °C | 239 °F | ISO 306 |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Vicat Softening Point | 115 - 129 °C | 239 - 264 °F | Average value: 124 °C Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Iran Petrochemical (PCC) 5218EA High Density Polyethylene HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed.. |
|||
Vicat Softening Point | 115 °C @Load 5.00 kg |
239 °F @Load 11.0 lb |
|
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Vicat Softening Point | 115 °C @Load 5.00 kg |
239 °F @Load 11.0 lb |
|
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® FXX210SK PBT+PC (Europe-Africa-Middle East) XENOY FXX210SK is an unreinforced PBT+PC injection moulding resin with excellent impact characteristics and containing a metal sparkle Visual FX. Applications: automotive bezels and appliances. XENO.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Vicat Softening Point | 115 °C | 239 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 115 °C | 239 °F | 50N; ISO 306 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 395A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |