Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 112 °C | 234 °F | B |
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i.. |
|||
Vicat Softening Point | 112 °C | 234 °F | B |
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg |
234 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity... |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | 1 kg; ASTM D1525 |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Vicat Softening Point | 112 °C | 234 °F | 1 kg; ASTM D1525 |
LG Chemical HP PMMA Information Provided by LG Chem |
|||
Vicat Softening Point | 112 °C | 234 °F | 50°C/h 50N |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Vicat Softening Point | 112 °C | 234 °F | ISO 306A |
Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
Vicat Softening Point | 112 °C | 234 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 112 °C | 234 °F | (50 °C/h / 50N) - B/50; ISO 306 |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Vicat Softening Point | 112 °C | 234 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 112 °C | 234 °F | VST/B/50; ISO 306 |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 112 °C | 234 °F | VST/B/50; ISO 306 |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 112 °C | 234 °F | 120°C / 10N; ISO 306 A 120 |
Styron EMERGEâ„¢ 7500 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7500 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Vicat Softening Point | 112 °C @Load 5.10 kg |
234 °F @Load 11.2 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525, ISO 306 |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ExxonMobil Method |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Vicat Softening Point | 112 °C | 234 °F | |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |
|||
Vicat Softening Point | 112 °C | 234 °F | |
Dow DOWLEX™ 2071 Linear Low Density Polyethylene DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Dow DOWLEX™ 2071D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Vicat Softening Point | 112 °C | 234 °F | |
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **) Injection molding grade, improved flow.Applications: Automotive industry: e.g. wheel trims, instrument panel components.Information provided by the manufacturer.Novodur is produced by Styrolution (2.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |