Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 105 °C | 221 °F | B |
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
Vicat Softening Point | 105 °C | 221 °F | 50°C/hr; 50N |
Polimeri Europa KOSTIL B366 Styrene Acrylonitrile Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-25 Injection moulding grade with good chemical resistance and easy flow grade Application fields: household.. |
|||
Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
Network Polymers NPS 80-0201 Crystal Polystyrene Description: Injection Molding Grade, High Heat ResistantInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Vicat Softening Point | 105 °C | 221 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® LX-0935 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 105 °C | 221 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
Rate A (50°C/h); ISO 306/B50; ASTM D1525 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Vicat Softening Point | 105 °C | 221 °F | ISO 306/A120 |
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in.. |
|||
Vicat Softening Point | 105 °C | 221 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 105 °C | 221 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SH 2114 High Impact Polystyrene Characteristics Very high impact strength Easy processing High heat Processing Extrusion MoldingApplications Toys, shoe heels, cosmetic boxes, pill vials Luggage cases Blending with clear polys.. |
|||
Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane Type: Estane® X595A-3FR TPU is a Shore 94A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Vicat Softening Point | 105 °C | 221 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP H 0560 GFCTG Polypropylene, 30% Mixed Filler PP homopolymer 30% mixed fillerGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C | 221 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Vicat Softening Point | 105 °C | 221 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Vicat Softening Point | >= 105 °C | >= 221 °F | At 1 kg |
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 105 °C | 221 °F | 10N (T° increase = 50°C/h); ASTM D1525A |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
Lucky EH-910 Acrylic, Extrusion Grade Highest heat and stress cracking resistance of Lucky PMMA grades. Recommended for extrusion of sheets, pipes, and profiles. Can also be used for injection molding of small parts. May be UV stabil.. |
|||
Vicat Softening Point | 105 °C | 221 °F | 50°C/h; 10N; 10x10x4mm; ISO 306/A50 |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |
|||
Vicat Softening Point | 105 °C | 221 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |