Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 103 °C | 217 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D648 |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Lendell Parapet GR-00100 PMMA, High Impact |
|||
Vicat Softening Point | 103 °C | 217 °F | 1000 g; ASTM D1525 |
LG Chemical 20HRE GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
Vicat Softening Point | 103 °C | 217 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Vicat Softening Point | 103 °C @Load 5.10 kg |
217 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution Absolac® 30GF15 ABS, 15% Glass Filled 15% glass filledInformation provided by Styrolution |
|||
Vicat Softening Point | 103 °C | 217 °F | (50 °C/h / 50N) - B/50; ISO 306 |
Styrolution Terblend® N NM-19 ABS/PA6 (Dry) Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL.. |
|||
Vicat Softening Point | 103 °C | 217 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Engineered Plastics EPABS 19 ABS Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Vicat Softening Point | 103 °C @Load 1.00 kg, Thickness 3.17 mm |
217 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 103 °C | 217 °F | |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de.. |
|||
Vicat Softening Point | 103 °C | 217 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Vicat Softening Point | 103 °C | 217 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Vicat Softening Point | 103 °C | 217 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Vicat Softening Point | 103 °C | 217 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Ineos Nova 5100 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold.. |
|||
Vicat Softening Point | 103 °C | 217 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Vicat Softening Point | 103 °C | 217 °F | ASTM D1525 |
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |
|||
Vicat Softening Point | 103 °C | 217 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL C443 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-25-20 Medium heat injection moulding grade. The availability of different industrial processes to manufa.. |
|||
Vicat Softening Point | 103 °C | 217 °F | 1 kg; ASTM D1525 |
LG Chemical HI835M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |