Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 99.0 °C | 210 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Vicat Softening Point | 99.0 °C | 210 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | 1000 g; ASTM D1525 |
LG Chemical SF-510 Alphalac Polystyrene
(Unverified Data**) Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | |
Ineos ABS LUSTROPAK® 1020 ABS, Extrusion Grade
(discontinued **) Extrusion grade.Applications: Food containers, blister packs.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority .. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Eastman M3019-P Polyethylene
(discontinued **) M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and.. |
|||
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 150 °C Grade Count:29 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
LyondellBasell Plexar® PX5335 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Ineos Nova 3101 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Vicat Softening Point | 99.0 °C @Load 5.00 kg |
210 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 99.0 °C @Load 5.00 kg |
210 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Vicat Softening Point | 99.0 °C @Load 5.10 kg |
210 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution Novodur® 250 ABS Novodur 250 is an injection molding grade of ABS with standard impact strength, high flow and high gloss.Information provided by Styrolution |
|||
Vicat Softening Point | 99.0 °C @Load 5.10 kg |
210 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
Vicat Softening Point | 99.0 °C | 210 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 98.9 °C @Load 1.02 kg |
210 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Stratasys® ABS-M30i ABS-M30i is a high strength material well suited for the medical, pharmaceutical
and food packaging industries. Parts manufactured with ABS-M30i material
are biocompatible (ISO 10993 certified) an.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP6415 High Gloss High Impact Polystyrene Characteristics Very good gloss with the retention of ESCR properties Good toughness Also available in various color shades Processing Injection moldingApplications Refrigerator end caps Refriger.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D648 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D-1525 |
Chevron Phillips MarFlex® 4553 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceLow coefficient of friction Applications: .. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Chevron Phillips MarFlex® 5430 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Excellent opticsEasy processingHigh coefficient of frictionTypical cast film applications include:OverwrapCoextruded filmGeneral purpose.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525-95 |
Multibase Multi-ABS 2925 FR Flame Retardant ABS Data provided by Multibase. |
|||
Vicat Softening Point | 98.9 °C | 210 °F | ASTM D648 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, High Flow Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525 |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Vicat Softening Point | 98.9 - 166 °C | 210 - 331 °F | Average value: 154 °C Grade Count:8 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Vicat Softening Point | 99.0 °C | 210 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface.. |