Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 93.9 °C | 201 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 51 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® GM 30 Low Density Polyethylene - Coating Grade Riblene GM 30 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 is suitable for coating applications where low neck-in and high manufacturing speed are req.. |
|||
Vicat Softening Point | >= 94.0 °C | >= 201 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 535 General Purpose Polystyrene Grade 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. It is used for electronic packaging, extruded light diffusers and office accessories.Informa.. |
|||
Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Eastman 1840A Polyethylene
(discontinued **) Polyethylene 1840A is a low-density formulation with no slip or antiblock. It is suggested for injection molding applications requiring good stiffness, gloss, good processability or layflat properti.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | 50°C/h 50N |
Ineos ABS Centrex® 811 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 94.0 °C | 201 °F | 50 N, 50°C/h; ISO 306 |
LG Chemical LI-913 ASA, Injection Molding, High Impact Information Provided by LG Chem |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Vicat Softening Point | 94.0 °C | 201 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.9 °C | 201 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRP 5608 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
UBE F222 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D-1525-95 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | |
Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging ap.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | |
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | 49 N; ISO 306 |
A.D. Compound Adene NCJA Homopolymer 30% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 94.0 °C | 201 °F | 49 N; ISO 306 |
A.D. Compound Adene NTFA Homopolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | >= 94.0 °C | >= 201 °F | At 1 kg; ASTM D1525 |
Iran Petrochemical (PCC) Tabriz WT1235 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | 50°C/h 50N |
Ineos ABS Centrex® 825 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
Vicat Softening Point | 94.0 - 115 °C | 201 - 239 °F | Average value: 100 °C Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Vicat Softening Point | 94.0 °C | 201 °F | ASTM D648 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |