Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 87.0 °C | 189 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Vicat Softening Point | 87.2 - 91.1 °C | 189 - 196 °F | ASTM D1525 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 87.0 °C | 189 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL PD H210/K ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | 50°C/hr; 50N |
Arkema Group Oroglas® HFI-7 Acrylic
(discontinued **) OROGLAS HFI-7 is a medium impact grade that in addition to the improvement in impact resistance provides superior flow which contribute to reduce the cycle time and improve demolding.Key features :.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 87.2 °C | 189 °F | ASTM D1525 |
Teknor Apex Laripur® LPR 9060EM Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | DSC; ASTM D3418 |
Westlake Tymax™ GT1057 Anhydride Modified Acrylate Copolymer Product Description: Westlake GT1057 is an anhydride modified low density polyethylene designed as an extrusion coating and laminating tie-layer. Westlake GT1057 provides excellent adhesion to pol.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | 50N-50°C per hour; ISO 306 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | 50N-50°C per hour; ISO 306 |
Total PPH 7062 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7062 is an antistatic homopolymer.ApplicationATOFINA Polypropylene PPH 7062 is intended for injection molding applications of boxes, closures and household articles. Inform.. |
|||
Vicat Softening Point | 87.0 °C @Load 5.10 kg |
189 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total PS CPDS 801 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 801 is a high impact brominated flame retardant polystyrene for use in injection molding and extrusion/thermoforming. PS CPDS 801 can be supplied in both natural an.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
UBE UMERIT 613A Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Dow 4010 Low Density Polyethylene (LDPE) Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Braskem BC 818 LDPE Extrusion Coating Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Extrusion coating. Information provided by Braskem |
|||
Vicat Softening Point | 87.0 °C | 189 °F | |
Eastman Tenite 105-23 Cellulose Acetate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 |
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print.. |
|||
Vicat Softening Point | 87.0 °C | 189 °F | ISO 306 |
Manifattura Cattaneo PP-s Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |