Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR N1841 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | >= 86.0 °C | >= 187 °F | At 1 kg; ASTM D1525 |
Iran Petrochemical (PCC) Tabriz 3630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 86.0 °C @Load 5.00 kg |
187 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Vicat Softening Point | 86.0 °C | 187 °F | resin; ASTM D1525 |
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-35 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Phr = 0 |
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | VST/A/50; ISO 306 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRF 3704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Eastman Spectar® Clear Copolyester for Thermoforming Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOd.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ISO 306 |
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade) Product Description: LD 615BA is a medium flow LDPE grade, characterized by high stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal S.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N; ISO 306 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | JIS-K-6740 |
Denka VINYKON R3201 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |