Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 60.0 °C | 140 °F | Rate B; ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | VST/B/50; ISO 306 |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ISO 306 |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ISO 306 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Vicat Softening Point | 60.0 °C @Load 5.00 kg |
140 °F @Load 11.0 lb |
|
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM-D1525 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50N-50°C per hour; ISO 306 |
Total PPC 3660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3660 is an heterophasic copolymer. PPC 3660 is characterized by a low fluidity hence good melt strength to provide east of processing and good manufactured article propert.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
DuPont Appeel® LSR20D751 Lidding Sealant Resin Appeel® LSR20D751 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 20D875 Ethylene Acrylate Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Vicat Softening Point | 60.0 °C @Load 5.10 kg |
140 °F @Load 11.2 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50 N - B method; ISO 306 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50°C/hr; 50N |
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Vicat Softening Point | 60.0 °C @Load 1.02 kg |
140 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem Evateno® 3019 PE EVA Foam Copolymer Evateno® 3019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. Evateno® 3019 PE is an easy processing and crosslinkable product with high compatibility with oth.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 60.0 °C @Load 5.00 kg |
140 °F @Load 11.0 lb |
|
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 60.0 - 143 °C | 140 - 289 °F | Average value: 122 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
Mitsui NOTIO™ PN-2070 Nano-crystal Structure Controlled Elastomer NOTIO™ is a polyolefin elastomer designed by a really new concept. NOTIO™ is a controlled crystal and amorphous structure on a nano scale, and shows better properties when compared with conventio.. |