Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 51.0 °C @Load 1.00 kg |
124 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® MQ F0 Very Low Density Polyethylene Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap.. |
|||
Vicat Softening Point | 51.0 - 97.8 °C | 124 - 208 °F | Average value: 81.7 °C Grade Count:67 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8120 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | ASTM D1525 |
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2207 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Vicat Softening Point | 51.1 °C | 124 °F | Peak Melting Temperature; ASTM D1525 |
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer. TC 110 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact s.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | |
Dow AFFINITY™ SM 8250 Polyolefin Plastomer AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex.. |
|||
Vicat Softening Point | 51.0 - 53.0 °C | 124 - 127 °F | ISO R 306 |
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding Beta and gamma resistant connectors |
|||
Vicat Softening Point | 51.0 °C | 124 °F | ISO 306 |
Arkema Group OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. ORE.. |
|||
Vicat Softening Point | 51.0 °C | 124 °F | B (50N); ISO 306 |
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe.. |