Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 255 - 263 °C | 491 - 505 °F | Average value: 262 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |