Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 88.0 °C @Load 1.00 kg |
190 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h.. |
|||
Vicat Softening Point | 88.0 °C @Load 1.00 kg |
190 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MP 20 Low Density Polyethylene - Injection Molding Riblene MP 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 20 are characterized by a high flexibility.Main Applications: Riblene MP 20 is suitable for injecti.. |
|||
Vicat Softening Point | 88.0 - 88.0 °C @Temperature 50.0 - 50.0 °C |
190 - 190 °F @Temperature 122 - 122 °F |
Average value: 88.0 °C Grade Count:1 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
Ineos Nova 5751 High Impact Polystyrene
(discontinued **) High flow, Good impact, USP Class VIApplications: Single service impact, Medical, Housewares, CompoundingProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwi.. |
|||
Vicat Softening Point | 88.0 - 99.0 °C | 190 - 210 °F | ISO 306A |
Ineos Nova 602 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
Eastman 808A Polyethylene
(discontinued **) Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from.. |
|||
Vicat Softening Point | 88.0 - 104 °C | 190 - 219 °F | Average value: 93.5 °C Grade Count:5 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
Hannam Chemical Hanalac 775 ABS, Extrusion Grade Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ISO 306 |
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE) Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r.. |
|||
Vicat Softening Point | <= 88.0 °C | <= 190 °F | II Preparation |
Sibur ABS 1030 (30,31) Molding Grade ABS Plastic With high fluidity of melting, thermal and light resistance for large parts of devices, parts of refrigerators, and for hearing aids. Mark is allowed for contact with food products. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 88.0 °C @Load 1.02 kg, Temperature 120 °C |
190 °F @Load 2.25 lb, Temperature 248 °F |
ASTM D1525 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TX-0510T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
UBE L719 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 1kg load; ISO 306 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1005 VL 2C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for thermal agricultural films to 180 at 200 µ with diffusing effect, for greenhouse coverage.ISO d.. |
|||
Vicat Softening Point | 88.0 - 104 °C | 190 - 219 °F | Average value: 95.9 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50N (T° increase = 5°C/h); ASTM D1525B |
Total Lacqrene® 814(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformati.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | 50°C/hr; 50N |
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse .. |
|||
Vicat Softening Point | 88.0 - 106 °C | 190 - 223 °F | ISO 306A |
Ineos Nova 610 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Vicat Softening Point | 88.0 °C | 190 °F | ASTM D1525 |
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinue 6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin.. |