Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 85.0 °C | 185 °F | B |
Plastcom SLOVALEN PC 51 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 1kg load; ISO 306 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Vicat Softening Point | 85.0 °C @Load 1.00 kg |
185 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin
(discontinued **) Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | resin; ASTM D1525 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D648 |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Vicat Softening Point | 85.0 - 117 °C | 185 - 243 °F | Average value: 104 °C Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | |
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
LyondellBasell Petrothene® NA952094 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50 N, 50°C/h; ISO 306 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Vicat Softening Point | 85.0 °C | 185 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total PS CPDS 818R Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 818R is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle ti.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1810/1811 Polystyrene 1811 is a very easy flowing crystal polystyrene designed, principally, for the injection molding industry. The excellent processing characteristics of this grade allows for the production of articl.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 1kg load; ASTM D1525 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 1kg load; ASTM D1525 |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 1kg load; ASTM D1525 |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | ASTM D1525 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | Loading 1, Rate A; ASTM D1525 |
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene appl.. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 85.0 °C @Load 0.999 kg |
185 °F @Load 2.20 lb |
ISO 306 |
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances .. |
|||
Vicat Softening Point | 85.0 °C | 185 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 85.0 - 107 °C | 185 - 225 °F | Average value: 94.4 °C Grade Count:156 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |