Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 70.0 °C @Load 1.00 kg |
158 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Radici Radilon® CS38 Copolyamide 6 semiaromatic Film extrusion gradeInformation provided by Radici group. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Radici Radilon® CS38FL (dry) Copolyamide 6 semiaromatic Film gradeInformation provided by Radici group. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latilub 45/7-20T HDPE, PTFE Reinforced Self-lubricating product based on High density polyethylene (HD-PE). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
SK Chemicals SKYTHANE® R180A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol Estane® T460AH Thermoplastic Polyurethane Type: Estane® T460AH is a Shore 60A, polyester grade, plasticizer-free, with low hardness and Hydrolytic Stabilizer thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: Americas, .. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | D1525 |
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength m.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 7760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7760 is a heterophasic copolymer. PPC 7760 is characterized by medium fluidity offering a combination of ease of processing and excellent impact properties in applications ranging.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol Estane® CR180A Thermoplastic Polyurethane Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | B (50N); ISO 306 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel Product Description: Vistamaxx 3020FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Vicat Softening Point | 70.0 °C @Load 0.999 kg |
158 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 10712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |
|||
Vicat Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 76.7 °C Grade Count:3 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |