Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 66.0 °C | 151 °F | 1000g; ASTM D-1525 |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ASTM D1525 |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ASTM D1525 |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | |
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ASTM D1525 |
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ISO 306B |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | B50 (50N); ISO 306 |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 66.0 - 68.0 °C @Load 5.00 kg |
151 - 154 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ART 0665/S Rigid PVC, Atoxic for General Purpose Injection moulding and blow moulding bottles |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR7060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | |
BASF Novolen® 2300 L Polypropylene Injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Vicat Softening Point | 66.0 °C | 151 °F | ASTM D1525 |
Arkema Group OREVAC® 9307 Y EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Vicat Softening Point | 66.0 - 113 °C | 151 - 235 °F | Average value: 97.4 °C Grade Count:34 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |