Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 61.0 °C @Load 1.00 kg |
142 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: .. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
DuPont Elvax® 3174 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film
(discontinued **) 18 wt% Vinyl Acetate.Elvax® 3174 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
DuPont Elvax® 3174SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in c.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer The Tritheva® PN 2021 resin is an Ethylene-Vinyl Acetate copolymer (EVA) mainly used for the production of crosslinked/expanded plates and other parts. This is an easy processing product with high .. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7610 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact streng.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
Vicat Softening Point | 61.0 °C | 142 °F | 1kg load; ASTM D1525 |
Micropol E188 Rotational molding powder based on a random EVA copolymer Information provided by Micropol Limited |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | ASTM D1525 |
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Vicat Softening Point | 61.0 °C @Load 1.02 kg |
142 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PN2021 EVA Foam Copolymer PN2021 is an Ethylene-Vinyl Acetate (EVA) copolymer mainly used for the production of crosslinked/expanded plates and other parts. It is a product with easy processability and high compatibility wit.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 61.0 °C @Load 0.999 kg |
142 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 8200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 82.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Vicat Softening Point | 61.0 °C | 142 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |