Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 60.0 °C @Load 1.00 kg |
140 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7010 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A; ISO 306 |
FKuR Kunststoff Bio-Flex® F 6510 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | VST/B/50; ISO 306 |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ISO 306 |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ISO 306 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Vicat Softening Point | 60.0 °C @Load 5.00 kg |
140 °F @Load 11.0 lb |
|
LATI Laticonther 83 CP/85 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Vicat Softening Point | 60.0 °C @Load 5.00 kg |
140 °F @Load 11.0 lb |
|
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Vicat Softening Point | 60.0 °C @Load 5.00 kg |
140 °F @Load 11.0 lb |
|
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM-D1525 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50N-50°C per hour; ISO 306 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525, ISO 306 |
DuPont™ Surlyn® E185SB Ionomer Resin Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed.. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50 N - B method; ISO 306 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | 50°C/hr; 50N |
Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It .. |
|||
Vicat Softening Point | 60.0 °C | 140 °F | ASTM D1525 |
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin
(discontinued **) ESCOR AT 310 provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier .. |
|||
Vicat Softening Point | 60.0 - 143 °C | 140 - 289 °F | Average value: 122 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |