Thermal Properties Metric English Comments
Vicat Softening Point 50.0 °C
122 °F
Rate A; ISO 306/A50
Premix Thermoplastics PRE-ELEC® CP 1316  (discontinued **)
PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Vicat Softening Point 50.0 °C
122 °F
1000g; ASTM D-1525
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca..
Vicat Softening Point 50.0 °C
122 °F
Rate A; ASTM D1525
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
DuPont Bynel® 21E553 Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Vicat Softening Point 50.0 °C
122 °F
Lucite International Elvacite ® 4400 Acrylic Resin
Elvacite® 4400 is a solid methacrylate copolymer bead resin designed for use in formulating thermosetting powder coating systems for exceptionally durable films. The resin may be used as the main..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide..
Vicat Softening Point 50.0 °C
122 °F
ASTM-D1525
Westlake EMAC® SP2409 20% EMA Copolymer
Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
DuPont Bynel® 1123 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Vicat Softening Point >= 50.0 °C

@Load 5.00 kg
>= 122 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP KUR 1010 TG05 Polypropylene, 5% Mineral Filled
PP copolymer 5% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 50.0 °C
122 °F
50°C/h 50N; ISO 306
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Vicat Softening Point 50.0 °C
122 °F
50°C/h 50N; ISO 306
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525 and ISO 306/A
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin
Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525, ISO 306
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525, ISO 306
DuPont™ Elvax® 3178Z Ethylene Vinyl Acetate
DuPont™ Elvax® 3178Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
ExxonMobil Polybilt™ Bitumen Modifier 106 Low Density Polyethylene Resin
Polybilt 106 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 106 content to achieve ..
Vicat Softening Point >= 50.0 °C

@Load 5.00 kg
>= 122 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP KUR 1520 TG05 Polypropylene, 10% Mineral Filled
PP copolymer 10% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525-82
Arkema Group Orevac® 18216 Maleic Anhydride modified EVA
Orevac® 18216 resin is a maleic anhydride modified ethylene - vinyl acetate copolymer designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between layers.Inf..
Vicat Softening Point 50.0 °C
122 °F
50°C/hr; 50N
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i..
Vicat Softening Point 50.0 - 210 °C
122 - 410 °F
Average value: 145 °C Grade Count:55
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Vicat Softening Point 50.0 - 155 °C
122 - 311 °F
Average value: 112 °C Grade Count:25
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Vicat Softening Point 50.0 °C

@Load 5.00 kg
122 °F

@Load 11.0 lb
LATI Latimass 53/11-02 D030 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Vicat Softening Point 50.0 °C

@Load 5.00 kg
122 °F

@Load 11.0 lb
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Vicat Softening Point 50.0 °C

@Load 5.00 kg
122 °F

@Load 11.0 lb
LATI Latimass 53-04 D009 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Vicat Softening Point 50.0 °C

@Load 5.00 kg
122 °F

@Load 11.0 lb
LATI Latiohm 52/11-10 PD02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Vicat Softening Point 50.0 - 129 °C
122 - 264 °F
Average value: 115 °C Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..
Vicat Softening Point 50.0 °C

@Load 5.00 kg
122 °F

@Load 11.0 lb
LATI Latistat 48/9900-03 EVA
Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..