Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 45.0 °C @Load 1.00 kg |
113 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | ASTM D1525 |
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: Flame Retardant: Balance of Properties (Impact, Mechanical and Heat)Applications: Computer, Monitor and Printer Housings, Microwave Co.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | 50 N; ISO 306 |
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | ASTM D1525 |
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | ISO 306/A |
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications Product Description: Exact 8210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications req.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | ASTM D1525 |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |
|||
Vicat Softening Point | <= 45.0 °C | <= 113 °F | ASTM D1525 |
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut.. |
|||
Vicat Softening Point | <= 45.0 °C | <= 113 °F | ASTM D1525 |
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in .. |
|||
Vicat Softening Point | 45.0 °C @Load 1.02 kg |
113 °F @Load 2.25 lb |
ASTM D1525 |
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly.. |
|||
Vicat Softening Point | 45.0 °C @Load 0.999 kg |
113 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam.. |
|||
Vicat Softening Point | 45.0 °C @Load 0.999 kg |
113 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de.. |
|||
Vicat Softening Point | 45.0 °C @Load 0.999 kg |
113 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des.. |
|||
Vicat Softening Point | 45.0 °C @Load 0.999 kg |
113 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | ASTM D1525 |
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | B (50N); ISO 306 |
Borealis Daplen™ EE103AE TPO Compound Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Vicat Softening Point | 45.0 - 95.0 °C | 113 - 203 °F | Average value: 73.0 °C Grade Count:13 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |
|||
Vicat Softening Point | 45.0 °C | 113 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |