Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 222 °C | 432 °F | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Vicat Softening Point | 222 °C | 432 °F | STN EN ISO 306 |
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to.. |
|||
Vicat Softening Point | 222 °C | 432 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Vicat Softening Point | 222 °C | 432 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Vicat Softening Point | 222 °C | 432 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Vicat Softening Point | 222 °C | 432 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate A/120; ISO 306 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP PF005 PA 6 (Europe-Africa-Middle East) 25% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
Vicat Softening Point | 222 °C | 432 °F | ISO 306 |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Vicat Softening Point | 222 °C | 432 °F | B/120; ISO 306 |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 222 °C | 432 °F | B/120; ISO 306 |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 222 °C | 432 °F | B/120; ISO 306 |
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 222 °C | 432 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |