Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 188 °C | 370 °F | Rate B; ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Vicat Softening Point | 188 °C | 370 °F | STN EN ISO 306 |
Plastcom SLOVAMID 6 HI-M PA6 with improved impact strength PA 6 with the content of thermoplastic elastomer. Impacted, for moldings with higher toughness even at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets, protecti.. |
|||
Vicat Softening Point | 188 °C | 370 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 188 °C | 370 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem LTX931A PEI Blend (Europe-Africa-Middle East) Post-industrial recycle based, 30% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 188 °C | 370 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 188 °C | 370 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Vicat Softening Point | 188 °C | 370 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Vicat Softening Point | 188 °C | 371 °F | |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Vicat Softening Point | 188 °C | 370 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P.. |