Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 174 °C | 345 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Vicat Softening Point | 174 °C | 345 °F | ASTM D1525 |
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang... |
|||
Vicat Softening Point | 174 °C | 345 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East) NORYL PKN4752 is a translucent, high heat PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food cont.. |
|||
Vicat Softening Point | 174 °C | 345 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Vicat Softening Point | 174 °C | 345 °F | ASTM D1525 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Vicat Softening Point | 174 °C | 345 °F | ASTM D1525 |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
Vicat Softening Point | 174 °C | 345 °F | ASTM D1525 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Vicat Softening Point | 174 °C | 345 °F | ASTM D1525 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |