Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525B |
SABIC PP 518P Polypropylene Homopolymer for Fiber Applications Product Description: PP 518P is a PP homopolymer with a broad molecular weight distribution intended for fiber extrusion applications.PP 518P has the following features:Consistent processabilityGoo.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525B |
SABIC PP 526P Polypropylene Homopolymer for Cast Film Product Description: PP 526P is specially developed for cast film applications for producing clear films and does not contain slip or antiblock additives.Films produced using PP 526P will exhibit:C.. |
|||
Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1310FRMA Polycarbonate Polycarbonate, General Purpose, Flame Retardant, UV StabilizedInformation provided by Ravago. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
PolyMirae Moplen HP420J BDDP Film Grade Polypropylene Moplen HP420J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP420J is a homopolymer particularly suitable for BOPP (Tender) fi.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
PolyMirae Moplen HP557G Stretch Grade Polypropylene Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container .. |
|||
Vicat Softening Point | 152 °C | 306 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® OQ3420 PC (Asia Pacific) Medium Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC H7500 Polypropylene, Homopolymer Features: Seetec H7500 is designed for the extrusion of continuous filament (CF). This grade is characterized by medium MWD and good processability from specific additives. SEETEC H7500 meets the FD.. |
|||
Vicat Softening Point | 152 °C @Load 1.00 kg |
306 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC H7700 Polypropylene, Homopolymer Features: Seetec H7700 is designed for the extrusion of fine fibers with the spunbond technology. This grade is characterized by very narrow molecular weight distribution (MWD), with anti-gas fading.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene Moplen Z 30 G is a high flow homopolymer for injection molding and compounding applications. Moplen Z 30 G exhibits a high stiffness and an outstanding processability for shorter cycle times and eas.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® BN-8110R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Vicat Softening Point | 152 °C @Load 5.10 kg |
306 °F @Load 11.2 lb |
Rate A (50°C/h); ISO 306/B50; ASTM D1525 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impa.. |
|||
Vicat Softening Point | 152 °C | 306 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 10N-50°C per hour; ISO 306 |
Total PPH 7060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7060 is homopolymer.ApplicationATOFINA Polypropylene PPH 7060 is intended for the injection molding of packaging containers, toys, domestic appliances, garden furniture and.. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 120 M20 Polypropylene Copolymer Low fluidity for extrusion or injectionInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 420 K24 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 522 N30 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | -1kg; ASTM D1525 |
Braskem CP 405 XP Injection Molding Polypropylene Applications: Caps for soft drinks. Information provided by Braskem |
|||
Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
Addiplast Addilene J 220 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® BS-8110R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Vicat Softening Point | 152 °C @Load 1.02 kg |
306 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem H 203 HOMO Polypropylene Homopolymer H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low .. |