Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East) LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 955A PC (Europe-Africa-Middle East) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A is available in transparen.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® LF-1025 PC, Unreinforced Anti-Abrasion Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 148 °C | 298 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® L-1225Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has slightly high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear colorApplications:Co.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525; ISO 360/B50 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Loading 1 (10N); ASTM D1525 |
Teknor Apex Sinpolene CPP1030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Vicat Softening Point | 148 °C | 298 °F | A (10 N); ISO 306 |
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio.. |
|||
Vicat Softening Point | 148 °C | 298 °F | ISO 306 |
Polyram RamTough RZ321G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Vicat Softening Point | 148 °C | 298 °F | ASTM D1525 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 10N-50°C per hour; ISO 306 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 10N-50°C per hour; ISO 306 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® 3208 Polycarbonate Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications, yields especially tough parts, better resistance to hot water.Information provided by Ba.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® KU 1-1242/1 Polycarbonate, High Impact High viscosity, impact modified grade with good toughness at low temperatures (dark colors only).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N |
Covestro Texin® 245 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® KU 1-1242 Polycarbonate, High Impact High viscosity, impact modified grade with good toughness at low temperatures (light colors only).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer.. |
|||
Vicat Softening Point | 148 °C | 298 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element.. |