Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 163R PC (Europe-Africa-Middle East) LEXAN 163R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 163R is available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 164H PC (Europe-Africa-Middle East) LEXAN 164H resin is a medium viscosity multi purpose grade, containing a release agent to ensure easy processing. It is FDA food contact compliant in limited colors. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 203 PC (Europe-Africa-Middle East) LEXAN 203 resin is a high viscosity multi purpose polycarbonate with UV stabilization pacakges. This grade is UL94-V2 rated with all color options. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® FXM173R PC UV stabilized PC in special effects colors. Metallic and pearlescent additives. Color may affect performance.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HPS4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® LR900G2 PC (Europe-Africa-Middle East) PC 20% GF Recycle Grade, Preliminary properties |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML3729 PC (Europe-Africa-Middle East) LEXAN ML3729 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
Vicat Softening Point | 145 °C | 293 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Vicat Softening Point | 145 °C | 293 °F | ASTM D1525 |
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet Paper match is a multi layer graphic sheet. The core layer is a high rigidity PP. The skin layers are high field polyolefine. The surface bonds easily to inks and have some absorbing capacity.Main a.. |
|||
Vicat Softening Point | 145 °C | 293 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 145 - 150 °C | 293 - 302 °F | 50 N, 50°C/h; ASTM D1525 |
Iran Petrochemical (PCC) PC 0712 Polycarbonate Suitable for molding and extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 145 °C @Load 5.00 kg |
293 °F @Load 11.0 lb |
|
LATI Latistat 87/28-06 PC Dissipative product based on Polycarbonate (PC). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Vicat Softening Point | 145 °C | 293 °F | ISO 306/B50 |
Styron CALIBREâ„¢ 302V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Vicat Softening Point | 145 °C | 293 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Vicat Softening Point | 145 °C @Load 5.10 kg |
293 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Structural foam• 10%.. |
|||
Vicat Softening Point | 145 °C @Load 5.10 kg |
293 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black Information provided by Eurotec® |
|||
Vicat Softening Point | 145 °C | 293 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform.. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXM163R PC (Europe-Africa-Middle East) PC with Visual Effect, UV-Stabilizer, Heat Stabilized, Opaque. Colour package may affect properties. Application testing always recommended. |
|||
Vicat Softening Point | 145 °C | 293 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |