Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 103R PC (Europe-Africa-Middle East) LEXAN 103R is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 103R is available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East) Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® OQ4820 PC (Europe-Africa-Middle East) LEXAN OQ4820 is a high viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard resins. Fields of application for this material are optical lenses, f.i. in sun glass.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East) LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Vicat Softening Point | 144 °C | 291 °F | |
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Vicat Softening Point | 144 °C | 291 °F | ISO 306 |
Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics PC0703R PC PC0703R resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.This data was supplied by SABIC-IP f.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics PC0703R PC PC0703R resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.This data was supplied by SABIC-IP f.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Vicat Softening Point | 144 °C | 291 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 144 °C | 291 °F | ASTM D1525 |
Styron Pulse® 2200BG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 144 °C | 291 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Vicat Softening Point | 144 °C | 292 °F | ASTM D1525 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 144 °C | 291 °F | |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Vicat Softening Point | 144 °C | 291 °F | |
Covestro Makrolon® 2458 Polycarbonate, Injection Grade Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Vicat Softening Point | 144 °C | 291 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Vicat Softening Point | 144 °C | 291 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Vicat Softening Point | 144 °C | 291 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Vicat Softening Point | 144 °C | 291 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Vicat Softening Point | 144 °C @Load 1.02 kg |
291 °F @Load 2.25 lb |
Rate B (120°C/h); ASTM D1525 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |