Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 163R PC (Europe-Africa-Middle East) LEXAN 163R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 163R is available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 164R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with b.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East) LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Vicat Softening Point | 143 °C | 290 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Vicat Softening Point | 143 °C | 290 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® FXG161R PC (Europe-Africa-Middle East) FXG161R is a Lexan PC Translucent Grade in our VisualFX Portfolio. The Grade was developed to meet the Aesthetic Differentiation requirements of today´s Customers. Color package may effect prop.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPS4 PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® LR180R PC (Europe-Africa-Middle East) LR180R is a medium viscosity,release containing multipurpose polycarbonate industrial gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® OQ3732 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized PC for ophthalmic lenses. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East) VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 955A PC Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East) LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Vicat Softening Point | 143 °C | 289 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Vicat Softening Point | 143 °C | 289 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Vicat Softening Point | 143 °C | 289 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer .. |
|||
Vicat Softening Point | 143 °C | 289 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 DW POM Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor.. |
|||
Vicat Softening Point | 143 °C | 289 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |