Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Vicat Softening Point | >= 130 °C | >= 266 °F | A, Influenced by the processing conditions. Proper conditions can lead to softening about 130°C; ISO 306 |
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Vicat Softening Point | 130 °C | 266 °F | ASTM D1525 |
Hyosung Topilene R701 PP R701 Injection Random CopolymerApplications:High transparent productISBM bottleCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
|
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Vicat Softening Point | 130 °C @Load 5.00 kg |
266 °F @Load 11.0 lb |
|
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East) Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® XL1339 PC+PET (Europe-Africa-Middle East) XENOY XL1339 is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XEN.. |
|||
Vicat Softening Point | 130 °C | 266 °F | ISO 306 |
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta.. |
|||
Vicat Softening Point | 130 °C | 266 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |
|||
Vicat Softening Point | 130 °C | 266 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS TM 35 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 130 °C | 266 °F | 50 N - B method; ISO 306 |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Vicat Softening Point | 130 °C | 266 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 375D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |