Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C7410 PC+ABS (Asia Pacific) Cycoloy* C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® EX58F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Vicat Softening Point | 106 °C | 223 °F | ASTM D648 |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Vicat Softening Point | 106 °C | 223 °F | 10 N - 120°C/h; ISO 306/A120 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Vicat Softening Point | 106 °C | 223 °F | |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Vicat Softening Point | 106 °C | 223 °F | ISO 306B |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Vicat Softening Point | 106 °C | 223 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 106 °C @Load 5.10 kg |
223 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Vicat Softening Point | 106 °C | 223 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 106 °C | 223 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 106 °C | 223 °F | A (10N); ISO 306 |
Borealis Himod™ FT3280 LDPE for Film Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Vicat Softening Point | 106 °C | 223 °F | ISO 306 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Vicat Softening Point | 106 °C | 223 °F | ASTM D1525 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Vicat Softening Point | 106 °C @Load 1.00 kg, Thickness 3.17 mm |
223 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 106 °C | 223 °F | |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Vicat Softening Point | 106 °C | 223 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Vicat Softening Point | 106 °C | 223 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Vicat Softening Point | 106 °C | 223 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Vicat Softening Point | 106 °C | 223 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Vicat Softening Point | 106 °C | 223 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |